The (GdxY(1-x))(2)O-3: Er3+, Yb3+ [x=0.0, 0.1, 0.5, 0.9, 1.0] phosphor samples with 0.5 mol% concentration of Er3+ and 3.0 mol% of Yb3+, have been prepared using combustion route. The effect of variation of composition on the morphology, crystallinity and photoluminescence characteristics of the material has been investigated. The samples were post-heated at a temperature 1200 degrees C, for 5 h. We find systematic color tunability from red to green with an increase of Gd2O3 content in Y2O3 lattice. Further, the post-heated samples show an enhancement of fluorescence intensity for more than fifteen times. The samples were characterized by X-ray diffraction (XRD), scanning electron microscope (SEM), photoluminescence measurement and Fourier transform infrared (FTIR) techniques in order to find out the structural changes in host lattice. An increase in crystallite size has been marked with increasing Gd content while FTIR analysis explains the reason of variation in the fluorescence of rare earth ions in different host matrices. (C) 2011 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据