4.7 Article

Effect of preheating treatment at 575 °C of green compacts on porous NiAl

期刊

JOURNAL OF ALLOYS AND COMPOUNDS
卷 492, 期 1-2, 页码 219-225

出版社

ELSEVIER SCIENCE SA
DOI: 10.1016/j.jallcom.2009.12.018

关键词

NiAl intermetallics; Porous materials; Preheating treatment

资金

  1. National Natural Science Foundation of China [20476106, 50721003, 20636020]
  2. National Natural Science Founds for Distinguished Young Scholar [50825102]
  3. 863 program [2006AA03Z511]
  4. Chinese Ministry of Education's 111 project [2009B623400]

向作者/读者索取更多资源

The effect of preheating treatment on NiAl compacts was systematically investigated. The preheating treatment of green compacts at 575 degrees C preserves their original shapes. The formation of porous NiAl alloys usually accompanies with the volume expansion due to the formation of Ni2Al3 during the preheating treatment. The pore structures of porous NiAl alloys strongly depended on the preheating duration. The volume expansion, porosity and the maximum pore size increased with prolonged preheating treatment duration. Whereas the maximum pore size of final product decreased with increased preheating treatment duration. It has been found that the pore structures especially the maximum pore size strongly depend on the volume expansion determined by the intensity of exothermic reaction from the preheating temperature to the finally sintering temperature. (C) 2009 Elsevier B.V. All rights reserved.