4.7 Article

Densification behaviour of pure molybdenum powder by spark plasma sintering

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.ijrmhm.2010.03.003

关键词

Molybdenum; Spark plasma sintering; Densification; Microstructure

向作者/读者索取更多资源

Pure molybdenum was sintered with SPS under various temperatures, external pressures and heating rates. The microstructure of the specimens representing the different sintering conditions was investigated by classical metallographic methods. The relative density, the microhardness and the chord length distribution were measured. Linear shrinkage, depending on time or temperature, was calculated from piston travel, which was recorded during sintering process. These results show that the main part of consolidation takes place during fast heating up. The densification behaviour is controlled mainly by sintering temperatures and applied pressure. The molybdenum powder was successfully consolidated by SPS in very short times. A relative density of 95% was reached by sintering temperatures of 1600 degrees C and external pressure of 67 MPa. (C) 2010 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据