Hot corrosion behaviors of a Cr13Ni5Si2-based metal silicide alloy in Na2SO4+25wt.% K2SO4 and Na2SO4+25wt.% NaCl molten salts

标题
Hot corrosion behaviors of a Cr13Ni5Si2-based metal silicide alloy in Na2SO4+25wt.% K2SO4 and Na2SO4+25wt.% NaCl molten salts
作者
关键词
-
出版物
INTERMETALLICS
Volume 18, Issue 3, Pages 324-329
出版商
Elsevier BV
发表日期
2009-08-29
DOI
10.1016/j.intermet.2009.08.004