期刊
INORGANIC MATERIALS
卷 48, 期 6, 页码 613-618出版社
MAIK NAUKA/INTERPERIODICA/SPRINGER
DOI: 10.1134/S0020168512060167
关键词
-
Barium titanate powders have been prepared by calcining barium titanyl oxalate precipitated by the Clabaugh and Merker processes, and their crystallization kinetics, morphology, and phase composition have been assessed. The results demonstrate that the Clabaugh process allows one to obtain powders with a low content of residual phases and tune the grain size (68-1935 nm) and crystal structure of barium titanate in wide ranges. The powders prepared through the Merker process have a narrower range of crystallite sizes (110-740 nm) and higher content of residual phases.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐